CLC 1.2316 is a prehardened mold steel with improved corrosion resistance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming and heat treating. Filing Code: SS-1176. Producer or source: Industeel USA, LLC.