Abstract

Sumitomo XA704 is an advanced alloy for ultra-supercritical boilers and other high temperature applications. This datasheet provides information on composition, and elasticity as well as fracture toughness and creep. It also includes information on corrosion resistance as well as forming and joining. Filing Code: SS-1175. Producer or source: Sumitomo Metal USA Corporation.