Abstract

ATI 332Mo is an austenitic stainless steel designed primarily to use as a material for automotive flexible connectors. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-1158. Producer or source: Allegheny Ludlum.