Abstract

AK Steel Nitronic 30 has good wet abrasion resistance, good resistance to aqueous and atmospheric corrosion, high strength, economy, and improved stress-corrosion cracking resistance over common 18-8 stainless steels. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming and joining. Filing Code: SS-1138. Producer or source: AK Steel Corporation.