CorroPlast is a hardened 400 series stainless steel used as a holder or base for plastic molds. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on heat treating and machining. Filing Code: SS-1123. Producer or source: Deutsche Edelstahlwerke GmbH.