Abstract

Sandvik T302 HS is a general purpose austenitic stainless steel with respect to corrosion resistance only in a spring temper for higher strength. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear and bend strength It also includes information on forming and heat treating. Filing Code: SS-1074. Producer or source: Sandvik Steel Company and Sandvik AB.