Abstract

NAS 64 is a duplex stainless steel with molybdenum for pitting and crevice corrosion resistance and a duplex microstructure for resistance to stress-corrosion cracking. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-1072. Producer or source: Nippon Yakin Kogyo Company Ltd.