Abstract

NAS 254N is a high performance corrosion resistance austenitic stainless steel with resistance to hot sea water. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-1064. Producer or source: Nippon Yakin Kogyo Company Ltd.