Abstract

Incoloy alloy 25-6HN is a 6% Mo superaustenitic stainless steel. It offers an excellent combination of strength, ductility, and resistance to corrosion by a variety of media at an economical price. It is readily formed and welded. The properties of the alloy are enhanced by its content of nitrogen. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming, machining, and joining. Filing Code: SS-1056. Producer or source: Special Metals Corporation.