DMV 928 is a nickel-base alloy with high alloying elements of chromium, molybdenum, and copper for excellent corrosion resistance in reducing and oxidizing media. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-1048. Producer or source: Mannesmann DMV Stainless USA Inc.