Sandmeyer alloy SSC-6MO is a stainless steel high in nickel and chromium with good corrosion resistance and ductility. The alloy has 6% Mo and good resistance to pitting with a pitting resistance equivalent number (PREN) of 48. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-1016. Producer or source: Sandmeyer Steel Company.