Abstract

CLC 18-10Nb is one of the basic grades of stainless steels. It is niobium bearing and, with its low carbon content, ensures better ductility and avoids intergranular corrosion even on welded pieces without water quenching. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength as well as fracture toughness and creep. It also includes information on forming, machining, and joining. Filing Code: SS-991. Producer or source: Industeel USA, LLC.