AL 332Mo alloy is an austenitic stainless steel with relatively high chromium and nickel levels for strength, and corrosion and oxidation resistance. The alloy contains a moderate addition of molybdenum for resistance to aqueous corrosion and of manganese for resistance to oxidation in air containing water vapor. A small amount of niobium (columbium) is added for resistance to sensitization and resultant susceptibility to intergranular corrosion. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and bend strength. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-989. Producer or source: Allegheny Ludlum.