Abstract

Sandvik 13C26 is martensitic stainless strip steel that has very good wear resistance. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on forming and heat treating. Filing Code: SS-951. Producer or source: Sandvik Steel Company.