Sandvik 7C27Mo2 is martensitic stainless strip steel that also contains molybdenum for corrosion resistance. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on forming and heat treating. Filing Code: SS-948. Producer or source: Sandvik Steel Company.