Abstract

DuraTech 20CV is a versatile tool steel that is highly wear resistant due to a large volume content of hard carbides. It is also corrosion resistant, with a high chromium content. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on corrosion resistance as well as forming, heat treating, machining, and powder metal forms. Filing Code: SS-947. Producer or source: Timken Latrobe Steel.