Abstract

Aluchrom Eco is an improved heating element material with extended life, especially in high-oxygen environments. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on corrosion resistance as well as forming and joining. Filing Code: SS-932. Producer or source: ThyssenKrupp VDM USA Inc.