Carpenter Stainless Type 304LN is a common, often used austenitic stainless steel. This data sheet emphasizes its use as rebar. This datasheet provides information on composition and physical properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-916. Producer or source: Carpenter Technology Corporation.