Abstract

NIROSTA 4318 is an austenitic stainless steel with good formability and with high mechanical properties due to the addition of nitrogen. The lower carbon content improves corrosion resistance when considering intergranular corrosion. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-883. Producer or source: ThyssenKrupp Nirosta GmbH.