Abstract

Staballoy 734 HS is an austenitic stainless steel with enhanced strength and corrosion resistance and is a stronger version of Staballoy 734 (see Alloy Digest SS-860, August 2002). This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as heat treating. Filing Code: SS-870. Producer or source: Allvac Ltd.