Abstract

Alloy 19D (UNS S32001), Nitronic 19D, is a lean duplex (ferritic-austenitic) stainless steel developed by AK Steel. Compared to conventional duplex and super-duplex stainless steels, alloy 19D has a reduced chromium content, man-ganese is substituted for most of the nickel, and molybdenum is essentially eliminated. Gibson Tube conducted a development program to produce seam-welded 19D tubing. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion resistance. Filing Code: SS-841. Producer or source: Gibson Tube.