Abstract

This austenitic stainless steel was designed with high silicon content to resist concentrated nitric acid. Typical applications are in explosives manufacturing. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as joining. Filing Code: SS-811. Producer or source: Allegheny Ludlum Corporation.