Abstract

Kubota alloy KHR20T is an iron-chromium-nickel cast alloy with microalloying additions that increase its strength to greater than that of HK40 from 871-982 C (1600-1800 F). This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on casting and joining. Filing Code: SS-740. Producer or source: Kubota Metal Corporation.