Type CF10SMnN is a 17Cr-8.5Ni-8Mn-4Si cast alloy with excellent galling resistance, cavitation-erosion resistance, high mechanical properties, and good castability. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance as well as casting and heat treating. Filing Code: SS-727. Producer or source: Various stainless steel casting companies.