Abstract

Allegheny Ludlum Type 310 is an austenitic chromium-nickel steel with high heat resisting properties. It is recommended for furnace equipment, heat treating boxes, burners, heat recovery systems, jet engine components, and heat exchangers. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture toughness, creep, and fatigue. It also includes information on corrosion resistance as well as forming and heat treating. Filing Code: SS-719. Producer or source: Allegheny Ludlum Corporation.