AL 800H and AL 800AT are nickel-iron-chromium alloys designed to resist oxidation and carburization at elevated temperatures. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-717. Producer or source: Allegheny Ludlum Corporation.