Remanit 4113 is an 18% Cr ferritic stainless steel with molybdenum added for improved corrosion resistance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: SS-697. Producer or source: Thyssen Stahl AG.