Abstract

Wiscalloy 25-35Nb is a high-temperature cast heat-resistant stainless steel with good creep-rupture properties. The alloy is centrifugally cast and is often used as petrochemical furnace tubing. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on casting and joining. Filing Code: SS-654. Producer or source: Wisconsin Centrifugal.