Abstract

Avesta Sheffield SAF 2507 is an austenitic/ferritic duplex stainless steel with very high strength. The alloy has a lower coefficient of thermal expansion and a higher thermal conductivity than austenitic stainless steels. The alloy has a high resistance to pitting, crevice, and general corrosion; it has a very high resistance to chloride stress-corrosion cracking. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-652. Producer or source: Avesta Sheffield Inc.