Abstract

Uranus 800 is employed at temperatures above 600 deg C (1112 deg F). This austenitic alloy offers good oxidation and creep resistance and is used frequently in petrochemical applications such as for reformers and ethylene crackers. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength as well as creep. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-650. Producer or source: Creusot-Marrel.