Abstract

REMANIT 4510 is a ductile non-hardenable type of stainless steel recommended for parts requiring a combination of good formability, weldability and corrosion resistance. This composition is a modification of Type 430 with an addition of titanium. This addition helps in corrosion resistance making the alloy useful in washing machines and hot water boilers. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance as well as forming, heat treating, and joining. Filing Code: SS-628. Producer or source: Thyssen Stahl AG.