Abstract

MAERKER G-4832 is a 20Cr-14Ni heat resistant casting for use in industrial furnaces. The alloy features good ductility and low embrittlement. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on casting and joining. Filing Code: SS-626. Producer or source: Schmidt & Clemens Inc.