Abstract

REMANIT 4509 was developed specially for silencers and exhaust gas purification plants. Due to its composition, this steel exhibits scale resistance up to 950 C and a high degree of corrosion resistance to the gases occurring in the exhaust system. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-613. Producer or source: Thyssen Stahl AG.