Abstract

PARALLOY CR32W is a cast austenitic high alloy stainless steel for applications to 1000 C (1180 F). The alloy balances high strength with good creep ductility. Typical applications include outlet headers and manifolds (pigtails) in steam methane reformers. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on high temperature performance as well as casting. Filing Code: SS-580. Producer or source: Paralloy Ltd.