Abstract

PYROWEAR 675 stainless is a corrosion resistant steel designed to be carburized for wear resistance while maintaining a ductile core. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on heat treating. Filing Code: SS-574. Producer or source: Carpenter.