Abstract

URANUS SB 8 is a super austenitic chromium nickel molybdenum and nitrogen alloy, 25.25.5 Cu type. This grade has been designed for high chloride environments. It is perfectly adapted to pulp and paper medias, stagnant sea water environments and for fabrications handling contaminated phosphoric acid. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-568. Producer or source: Creusot-Marrel.