REMANIT 4439 is a highly corrosion resistant steel with low carbon content, an addition of nitrogen to enhance both mechanical properties and corrosion resistance, and higher molybdenum than most stainless steels to resist pitting and crevice corrosion in chloride media. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-556. Producer or source: Thyssen Stahl AG.