Abstract
CRONIFER 2418 MoN AND 2419 MoN are austenitic stainless steels with an excellent combination of corrosion resistance and very high strength. A special grade of 2418 MoN meets UNS S34565. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-546. Producer or source: VDM Technologies Corporation.