AVESTA 353 MA is a high-temperature austenitic stainless steel with excellent scaling resistance, creep strength at elevated temperatures, with carburization and nitriding resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-532. Producer or source: Avesta Stainless Inc..