Abstract

REMANIT 4565S is a fully austenitic stainless steel which features both high strength and excellent corrosion resistance in a wide range of corrosive media. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as forming and heat treating. Filing Code: SS-529. Producer or source: Thyssen Specialty Steels Inc..