Abstract

UNS S31600 is an austenitic stainless steel with improved resistance to general corrosion and to pitting and crevice attack by virtue of its molybdenum content. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-514. Producer or source: Stainless steel mills.