Abstract

AVESTA 25-22-2LN is a stronger, more corrosion resistant austenitic stainless than AVESTA 17-15-2.5L (revised as AvestaPolarit 724L, Alloy Digest SS-501, October 2001). It is designed for use in equipment subject to the most corrosive conditions encountered in the production of urea. At 570 F (300 C) it has about a 35% higher yield strength than 17-15-2.5L. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as heat treating, machining, and joining. Filing Code: SS-506. Producer or source: Avesta Stainless Inc..