Abstract

INCOLOY Alloy DS is a wrought, austenitic nickel-chromium-iron alloy with high resistance to heat and oxidation. Its many applications include furnace parts, woven-wire conveyor belts for continuous furnaces, radiant heat tubes and gas-turbine components. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: SS-473. Producer or source: Inco Alloys International Inc..