Abstract

AVESTA STAINLESS 25L is a low-carbon austenitic stainless steel which possesses very high resistance to general and intergranular corrosion in strongly oxidizing environments such as nitric acid. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-464. Producer or source: Avesta Stainless Inc..