Abstract

NICROFER 3127 LC is a fully austenitic extra-low-carbon stainless steel to which has been added approximately 3% molybdenum and 1% copper. It is characterized by (1) Good resistance to general corrosion, (2) Excellent resistance to pitting, crevice and intergranular corrosion and to stress-corrosion cracking, and (3) Good mechanical properties. Its many uses include equipment for producing phosphoric acid by the wet method, equipment for handling sulfuric acid contaminated with chlorides, handling seawater and use in deep sour gas wells. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-446. Producer or source: Vereingte Deutsche Metallwerke AG.