CRUCIBLE 3041 is a non-hardenable, low-carbon austenitic chromium-nickel steel designed for special applications. It is particularly suitable for applications requiring welding operations where it is not practical to anneal alter welding. This grade is non-magnetic in the annealed condition but slightly magnetic when cold worked. Typical applications are screw machine products and all machined parts requiring good corrosion resistance or non-magnetic properties. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as heat treating, machining, and joining. Filing Code: SS-421. Producer or source: Crucible Specialty Metals Division, Colt Industries.