TECHALLOY A-286 is recommended for applications requiring high strength and good resistance to corrosion at temperatures up to 1300 F and for lower stresses at higher temperatures. Its oxidation resistance is high for continuous service to 1500 F and intermittent service to 1800 F. It is ideal for fasteners and other cold-headed parts and it provides good spring properties at high temperatures in corrosive environments. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, and tensile properties as well as creep and fatigue. It also includes information on low and high temperature performance as well as heat treating, machining, joining, and surface treatment. Filing Code: SS-365. Producer or source: Techalloy Company Inc..