Abstract

UCAR 302 is a cryogenically processed stainless steel wire with the same composition as AISI Type 302. The processing gives tensile and torsional properties that are independent of wire diameter and markedly greater than those of conventional stainless steels. UCAR 302 has uniformly high properties: 290,000 psi tensile strength and 145,000 psi minimum torsional yield strength. Thus it provides greater design flexibility than conventional stainless steels. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion resistance as well as forming, machining, joining, and surface treatment. Filing Code: SS-354. Producer or source: AL Tech Specialty Steel Corporation.