Abstract

CARPENTER STAINLESS 22Cr-13Ni-5Mn has very good corrosion resistance in combination with high strength. It has better corrosion resistance than AISI Type 316 stainless steel and approximately twice the yield strength. Carpenter 22Cr-13Ni-5Mn can be machined, cold worked and welded using the same equipment and methods used for the conventional AISI 300 series of stainless steels. It is nonmagnetic as annealed and after severe cold work. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-353. Producer or source: Carpenter.