Abstract

Carpenter 430FR Solenoid Quality stainless steel is a ferritic chromium-iron alloy developed especially for A.C. and D.C. magnetic circuit applications such as solenoid valve core components and electromagnetic relay cores. The electrical resistivity of 430FR is approximately 25% higher than other commercially available 430F stainless. Increased electrical resistivity provides better performance of magnetic components, particularly at power frequencies and high magnetic flux density. This datasheet provides information on composition, physical properties, and hardness. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-337. Producer or source: Carpenter.